I have made several prints on my photon plus at 50 micron layer thickness and have run into the first few layers being distorted. I imagine it’s because of the z-lift speed, minimal support structure, and a very thin layer height. Most of the resin exposure data out there is for 50 micron layer heights. Does anyone have data for 100 micron layer heights or a formula to increase know exposure times?
  
  
   
    翻譯年糕
   
   
   
  
 
						
										
					
						 Nick Williams
						Nick Williams
						2019-09-21 02:49:14
					
					
				 
				
					
						 Scott Pavlich
						Scott Pavlich
						2019-09-21 02:53:06
					
					
				 
				
					
						 Ray Regan
						Ray Regan
						2019-09-21 22:58:17
					
					
				 
				
					
						 Ray Regan
						Ray Regan
						2019-09-21 23:00:48